DOWSIL 1-4174

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL 1-4174

Main features

  • Controlled 180 um Bondline
  • 1.8 W/(m K) Thermal Conductivity
  • 20-Minute Cure at 150 deg C

Product Description

DOWSIL 1-4174 Thermally Conductive Adhesive is a one-part, gray silicone adhesive for bonding and transferring heat between electronic components and thermal-management hardware. The self-leveling, self-priming material uses 180 um glass spacer beads for bondline control. Cure schedules are 90 minutes at 100 deg C, 30 minutes at 125 deg C, or 20 minutes at 150 deg C. Typical thermal conductivity is 1.8 W/(m K), and typical unprimed aluminum lap shear is 4.5 MPa. Applications include integrated circuits, lids and housings, baseplates, and heat sinks.

Key features

  • Glass-bead bondline control: Embedded 180 um glass spacer beads control adhesive bondline thickness.
  • Thermal conductivity: Typical thermal conductivity is 1.8 W/(m K).
  • Elevated-temperature cure: The shortest listed cure schedule is 20 minutes at 150 deg C.

Applications

Bonding and sealing integrated circuits, lids and housings, baseplates, and heat sinks where thermal transfer is required.

Technical Specifications

General Properties
Color
The color
Gray
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.71
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
3.7
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
62,300 mPa.s
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
16 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.9 E+14 Ohms⋅cm
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.78 W/m.K

Additional Information

One-Part Thermally Conductive Adhesive

DOWSIL™ 1-4174 One-Part Thermally Conductive Adhesive

DOWSIL™ 1-4174 is a one-part, gray, thermally conductive silicone adhesive formulated for electronic assemblies and thermal management applications. The adhesive can flow, fill, or self-level after dispensing without requiring the mixing of separate components. Its temperature-controlled heat-curing process produces no cure by-products, supporting uniform cure in deep sections and confined assemblies.

With a typical cured thermal conductivity of 1.78 W/mK and the ability to achieve thin bond line thicknesses, DOWSIL™ 1-4174 helps transfer heat away from electronic devices. Its 7 mil glass bead technology supports controlled bond line thickness, while its cured mechanical and electrical properties make it suitable for consideration in electronic bonding applications.

1.78 W/mK thermal conductivity 7 mil glass bead technology One-part heat cure UL 94 V-0 classification
DOWSIL 1-4174 one-part gray thermally conductive silicone adhesive
One-part thermally conductive silicone adhesive for electronic assembly applications
Key Features & Benefits

Thermal Performance, Bonding Strength & Processing Flexibility

DOWSIL™ 1-4174 combines thermal conductivity with adhesive bonding and temperature-controlled curing. Its one-part formulation and cured properties support the integration of thermal management and mechanical attachment within electronic assemblies.

High Thermal Conductivity
Typical thermal conductivity of 1.78 W/mK supports heat transfer away from heat-generating electronic components.
Controlled Bond Line Thickness
7 mil glass bead technology helps maintain a uniform and controlled bond line thickness. Thin bond lines can help reduce thermal resistance and improve heat transfer.
One-Part Heat-Cure Formulation
Eliminates the need for component mixing. The adhesive can flow, fill, or self-level after dispensing, with curing controlled by temperature.
Strong Adhesion
Typical lap shear strength of 4.5 MPa on an aluminum substrate supports adhesive bonding. The formulation is designed to provide unprimed adhesion to many reactive metals, ceramics, and glass, as well as selected laminates, resins, and plastics.
Electrical Insulation & Flammability Classification
The cured adhesive has a typical dielectric strength of 400 V/mil and a UL 94 V-0 flammability classification.
Uniform Cure in Confined Assemblies
The addition-cure silicone formulation produces no cure by-products, allowing curing in deep sections and completely confined assemblies.
Recommended Applications

Where DOWSIL™ 1-4174 Fits

DOWSIL™ 1-4174 is highly recommended for a range of electronic assembly bonding applications, including the attachment of components and structures involved in thermal management.

Printed circuit board assembly application
Recommended for printed circuit board assemblies requiring thermally conductive adhesive bonding. The silicone formulation combines heat transfer capability with cured mechanical and electrical properties.
Integrated circuit substrate with a ball grid array (BGA) beside a microchip mounted on a green printed circuit board.
Bonding Integrated Circuit Substrates
Recommended for bonding integrated circuit substrates where adhesive attachment and thermal management are part of the electronic assembly requirements.
Exploded view of an electronic housing with a yellow lid, gray bonding frame, and ceramic base showing internal circuitry.
Adhering Lids & Housings
Suitable for consideration when adhering lids and housings in electronic assemblies. The adhesive provides thermal conductivity and mechanical bonding in a one-part heat-cure formulation.
Base plate attachment application
Base Plate Attachment
Recommended for base plate attachment applications where thermally conductive bonding and controlled bond line thickness are relevant to the assembly design.
Gray thermal adhesive being applied to a circuit board chip beneath an aluminum heat sink.
Heat Sink Attachment
Recommended for heat sink attachment, combining adhesive bonding with thermal conductivity to help transfer heat away from electronic devices.
Technical Specifications

Typical As-Supplied & Cured Properties

Typical As-Supplied Properties

Property Typical Value Method / Condition
Color Gray As supplied
Viscosity 62,300 cP Typical uncured value
Thixotropy 3.7 Typical uncured property
Specific Gravity 2.71 Uncured material
Heat Cure Time 90 mins 100°C
Heat Cure Time 30 mins 125°C
Heat Cure Time 20 mins 150°C
Rheometer T90 Cure Time 6.2 min 125°C

Typical Cured Properties

Property Typical Value Method / Condition
Thermal Conductivity 1.78 W/mK Typical cured property
Lap Shear Strength 4.5 MPa Aluminum substrate
Durometer Hardness 92 Shore A Cured material
Dielectric Strength 400 V/mil Electrical property
UL Flammability UL 94 V-0 Classification
The product description also expresses dielectric strength as 16 kV/mm. The tabulated value is 400 V/mil; these are approximately equivalent unit presentations after rounding.
Processing & Curing

Temperature-Controlled Heat-Cure Processing

DOWSIL™ 1-4174 contains all ingredients required for cure. The addition-cure silicone process is initiated by heat and can be accelerated by increasing the curing temperature. The formulation provides a long working time before cure initiation and produces no cure by-products.

Typical Heat-Cure Schedule

100°C (212°F)
90 minutes
125°C (257°F)
30 minutes
150°C (302°F)
20 minutes
Rheometer T90: 6.2 minutes at 125°C. This rheometer measurement is distinct from the typical heat-cure schedule listed above.

Application & Curing Instructions

  1. Apply the adhesive to the prepared substrate and assemble the components.
  2. Heat cure at 100°C (212°F) or higher to initiate the addition-cure silicone curing process.
  3. Use higher curing temperatures when faster processing is required, following the applicable cure schedule.
  4. For thin bond lines of less than 20 mils, cure for approximately 15 minutes at 150°C (302°F).
  5. For thicker sections, perform a pre-cure at 70°C (158°F) to help minimize void formation.
  6. Use 30 minutes at 70°C (158°F) as a starting pre-cure condition, then optimize according to section thickness and the degree of confinement.
  7. Complete the final heat cure to achieve full adhesive properties and uniform curing throughout the material.

Cure Characteristics

  • Contains all ingredients required for cure.
  • Produces no cure by-products.
  • Suitable for deep-section and confined applications.
  • Cures uniformly throughout the adhesive.
  • Provides a long working time before cure initiation.
Substrate Compatibility

Adhesion to Common Substrates

DOWSIL™ 1-4174 is formulated to provide unprimed adhesion to many reactive metals, ceramics, and glass, as well as selected laminates, resins, and plastics. The supplied substrate guidance also identifies epoxy laminate boards, reactive materials, and filled plastics among suitable substrate categories. Adhesion depends on substrate characteristics, and good adhesion is generally not expected on non-reactive metal surfaces or non-reactive plastics such as PTFE, polyethylene, and polypropylene.

Substrate Type Typical Adhesion Expectation
Reactive metals Good unprimed adhesion
Ceramics Good unprimed adhesion
Glass Good unprimed adhesion
Selected laminates Good adhesion
Selected resins Good adhesion
Selected plastics Good adhesion
Non-reactive metals Adhesion may be limited
Teflon™ (PTFE) Adhesion may be limited
Polyethylene Adhesion may be limited
Polypropylene Adhesion may be limited

Substrate Testing & Improving Adhesion

Substrate Testing

The guidance identifies 100 percent cohesive failure of the adhesive in a lap shear or similar adhesive strength test as the criterion for maximum bond strength and substrate compatibility assessment.

Testing can also help determine minimum cure time and identify surface contamination from mold release agents, oils, greases, and oxide films.

Surface Treatment

Difficult or non-reactive substrates may benefit from chemical etching or plasma treatment to create a more reactive surface and promote adhesion.

Primer Application

A Dow primer may be used to increase the chemical activity of difficult substrates.

  • Apply a very thin, uniform coating.
  • Wipe off excess primer.
  • Allow the primer to cure thoroughly before applying the silicone elastomer.
Cure Optimization & Validation

Increasing the cure temperature and/or cure time may improve ultimate adhesion where necessary. Conduct a small-scale laboratory evaluation of the substrate before proceeding to production trials.

Storage & Handling

Storage Instructions & Temperature Considerations

Original Packaging & Contamination Prevention

Store DOWSIL™ 1-4174 in its original packaging with the cover tightly attached to avoid contamination.

Product Label & Expiration Date

Follow any special storage instructions listed on the product label. Use the product by the indicated Expiration Date shown on the label.

Service Temperature Considerations

Silicone adhesive performance at temperature extremes depends on the application, component configuration, stress sensitivity, cooling rates, hold times, and prior temperature history. Thermal cycling performance should be verified for the intended parts or assemblies.

At elevated temperatures, the durability of the cured silicone elastomer is dependent on both time and temperature.

Next Steps

Review DOWSIL™ 1-4174 for Your Electronic Assembly

Share your electronic assembly requirements, substrate materials, target bond line thickness, curing conditions, and thermal management needs to discuss the suitability of DOWSIL™ 1-4174 for your application.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers