LOCTITE ABLESTIK NCF 234

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

LOCTITE ABLESTIK NCF 234

Main features

  • Non-conductive Underfill Film
  • Enable fine pitch, narrow gap Cu Pillar
  • Pb-free & low κ

Product Description

LOCTITE ABLESTIK NCF 234 transparent film is specially formulated for Pb free, low κ, thin gap, large and thin die used in advance flip chip applications. NCF 234 is suitable for die to die, die to wafer (TSV) or die to substrate applications.

Product Family

233995

330mm × 10m Roll - 2556995
1. Select Length
2. Select Package Type

Loading pricing…

Product availability
US Shipping in 48 days
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Roll
Net weight 11.4 g
Gross weight 46.4 g
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
34 µm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
105 °C

Additional Information

Thawing

  •  Allow container to reach room temperature before use, normally 30 minutes.

Recommended Cure Schedule

  • 30 minutes ramp to 175ºC, hold 2 hours @ 175°C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers