3M™ Dual Lock™ Reclosable Snap Tape SJ3550CF

Harmonization Code : 3926909790 |

3M™ Dual Lock™ Reclosable Snap Tape SJ3550CF

Main features

  • Black, interlocking mushroom-shaped heads (250 stem density per square inch)
  • Mates with Type 170, Type 250 or Type 400 stem densities
  • Clear, acrylic, tape bonds well to a variety of substrates

Product Description

3M™ Dual Lock™ Reclosable Fastener SJ3550CF is a durable, high-strength fastening system designed as a reliable alternative to traditional mechanical fasteners such as screws, nuts, and bolts. It features interlocking mushroom-shaped heads with a clear acrylic adhesive backing, allowing strong bonding to a wide range of substrates including metals, glass, and plastics. The fastener delivers a secure, reclosable solution with a distinctive audible snap that confirms proper engagement.

Product Key Features

  • Interlocking mushroom-shaped stems provide a secure bond that can be opened and closed repeatedly
  • 250 Stem Density: Balanced strength and ease of separation for versatile use
  • Bonds well to metals, glass, and plastics such as acrylic, polycarbonate, and ABS
  • Audible Snap Closure: Confirms proper fastening and secure engagement
  • Offers strong, durable adhesion with a clean appearance
  • Mates with Type 170, 250, or 400 stem densities for customized performance
  • Eliminates the need for drilling or hardware

Applications

  • Replacing screws, bolts, and other mechanical fasteners
  • Mounting panels, covers, and access components
  • Securing display systems and signage
  • Attaching components in electronics, appliances, and assemblies
  • Applications requiring repeated attachment and removal
  • Bonding to metal, glass, and rigid plastic surfaces
Product Family

234939

Black, 19 mm x 45.7 m, 5.7 mm, 40 cups/cm²
1. Select Width
2. Select Length
3. Select Thickness
4. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Roll
Net weight 2.045 kg
Gross weight 2.045 kg
Dimensions 26.5 x 26.5 x 7 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
5740 μm

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers