3M DP8810NS

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M™ Scotch-Weld™ Low Odor Acrylic Adhesive DP8810NS

Main features

  • Toughened
  • Excellent shear strength
  • High peel and impact strength

Product Description

3M™ Scotch-Weld™ DP8810NS Low Odor Acrylic Adhesive is a high performance, two-part acrylic adhesive that offer excellent shear, peel, and impact performance. DP8810NS provides improved adhesion to many plastics and metals, including those with slightly oily surfaces. It also features a fast rate of strength build, providing structural strength in minutes. The low odor and non-flammability features also make them easier to incorporate into a manufacturing process.

DP8810NS Green has been tested for surface flammability, smoke, toxic gas generation, and caloric content per ASTM E162, ASTM E662, ASTM E1354, Bombardier SMP 800-C, and Boeing BSS 7239 test methods.

Product Key Features

  • Toughened
  • Excellent shear strength
  • High peel and impact strength
  • 10:1 mix ratio control bond line thickness
  • Variety of open times available
  • Increased cure speed with applied heat
  • Contain glass beads (0.010” diameter) to control bond line thickness

Applications

  • Bonding metals such as aluminum, steel, and stainless steel
  • Adhesion of plastics including ABS, acrylics, polycarbonate, and PVC
  • Assembly of transportation components (rail, bus, automotive, aerospace interiors)
  • Structural panel bonding and composite assembly
  • Signage, display, and general industrial fabrication
  • Bonding dissimilar materials where minimal surface preparation is preferred
  • Applications requiring fast fixturing and high impact resistance
Product Family

204619

45 mL - Cartridge | Green
1. Select Color
2. Select Package Type

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Cartridge
Net weight 79.72 g
Gross weight 79.75 g
Dimensions 11.7 x 4.8 x 1.9 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Off-White/Blue
Density (g)
1.06 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
10:1
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
0.2 hours
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
45,000 mPa.s

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers