3M™ Scotch-Weld™ Acrylic Adhesive DP8507NS

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Acrylic Adhesive DP8507NS

Main features

  • Toughened
  • 10:1 mix ratio
  • Excellent shear strength on bare metals, plastics and other materials

Product Description

3M DP8507NS is a high-performance, two-part structural acrylic adhesive with excellent shear performance. It provides excellent shear strength on many plastics and metals, including good strength on metals with slightly oily surfaces. This special formulation allows the bonding of various metal substrates including cold-rolled steel, copper, brass, stainless steel and galvanized steel.

Product Features

  •  Excellent shear strength on bare metals, plastics and other materials
  • Toughened
  • 10:1 mix ratio
  • Contains ceramic particles to control bond line thickness

Applications

  • Bonding metal substrates including steel, stainless steel, and galvanized steel
  • Assembly of metal components in industrial and manufacturing environments
  • Fabrication of HVAC systems, enclosures, and sheet metal assemblies
  • Bonding of plastics to metals in multi-material designs
  • General industrial bonding where high shear strength is required
  • Applications involving slightly oily or minimally prepared metal surfaces
  • Structural bonding in transportation, appliances, and equipment manufacturing
Product Family

234880

490 ml Duo-Pak
1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Cartridge
Net weight 0.825463 kg
Gross weight 0.825463 kg
Dimensions 22 x 9.5 x 5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Off-White/Light Tan
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
10:1
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
0.12 hours
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
93000 mPa.s

Leading Brands Trust in Our Products and Services