3M Electrically Conductive Double-Sided Tape 9793KW Series

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M Electrically Conductive Double-Sided Tape 9793KW Series

Main features

  • 0.02-0.20 ohm under 3M ETM-12 test conditions
  • Typical expected shielding effectiveness of 40-60 dB
  • Broad thickness and adhesion selection

Product Description

3M-9793KW is an XYZ-axis electrically conductive double-sided pressure-sensitive adhesive tape that combines acrylic adhesive with a conductive matrix carrier. It provides an adhesive electrical path between joined substrates for grounding and EMI shielding in equipment and electronic components. The conformable, compressible construction is offered in twelve variants from 150 to 800 µm, with transparent PET liner configurations that vary by thickness. Product selection should consider thickness, adhesion target, liner configuration, surface condition, and the pressure needed to develop adhesive contact and electrical connection.

Key features

  • XYZ-axis conductivity: Z-axis electrical resistance is 0.02-0.20 Ω under 3M ETM-12 test conditions.
  • EMI shielding performance: Typical expected shielding effectiveness is 40-60 dB through the tape thickness using standard EMI shielding test methods.
  • Conductive construction: Acrylic PSA with a conductive matrix carrier combines pressure-sensitive attachment with electrical conductivity.
  • Thickness selection: Twelve variants are available from 150 to 800 µm.
  • Adhesion targets: Face-side targets range from 1200 to 2500 gf/inch and back-side targets from 1600 to 2500 gf/inch to stainless steel under ASTM D1000.

Applications / Suitable for

  • Grounding between conductive substrates.
  • EMI shielding in equipment and electronic components.
Product Family

234982

9793KW-400 | 480mm × 50m
1. Select Width
2. Select Length
3. Select Version

Loading pricing…

Packaging
Please select Width, Length and Version.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
Acrylic adhesive with conductive matrix
Color
The color
Grey Metallic
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
Transparent PET Liner

Additional Information

Electrically Conductive Tape

3M-9793KW

3M-9793KW is an XYZ-axis electrically conductive double-sided pressure-sensitive adhesive tape that combines acrylic adhesive with a conductive matrix carrier. It provides adhesive attachment and a conductive path between substrates for grounding and EMI shielding in equipment and electronic components. Twelve thickness variants from 150 to 800 µm provide options for different assembly geometries and gap conditions.

XYZ-axis electrical conductivity Double-sided acrylic PSA Compressible conductive matrix 12 thickness variants: 150-800 µm

3M-9793KW electrically conductive double-sided pressure-sensitive adhesive tape.

Product construction

Construction and as-supplied characteristics

Construction
Acrylic PSA + conductive matrix carrier
The double-sided conductive construction combines pressure-sensitive attachment with an electrical path through the tape.
Color
Grey metallic
The face and back sides are both listed as grey metallic.
Release liner
Transparent PET
Variants at 400 µm and thinner use dual liners; 450 µm and thicker variants use a single liner.
Standard roll format
1050 mm x 100 m
The series is listed as available in this roll size.

Thickness, adhesion and liner options

The 9793KW series is offered in twelve thickness variants from 150 to 800 µm. Adhesion target values to stainless steel vary by thickness, and liner configuration changes at 450 µm. Values below are representative/typical and are not specification limits.

Variant Thickness (µm) Face-side adhesion to SUS (gf/inch) Back-side adhesion to SUS (gf/inch) Liner configuration
9793KW-150 150 1200 1600 Dual transparent PET liner
9793KW-200 200 1600 1600 Dual transparent PET liner
9793KW-250 250 1600 1600 Dual transparent PET liner
9793KW-300 300 2000 2000 Dual transparent PET liner
9793KW-350 350 2000 2000 Dual transparent PET liner
9793KW-400 400 2000 2000 Dual transparent PET liner
9793KW-450 450 2000 2000 Single transparent PET liner
9793KW-500 500 2000 2000 Single transparent PET liner
9793KW-550 550 2000 2000 Single transparent PET liner
9793KW-600 600 2000 2000 Single transparent PET liner
9793KW-650 650 2000 2000 Single transparent PET liner
9793KW-800 800 2500 2500 Single transparent PET liner

Thickness and adhesion values are reported using ASTM D1000. Adhesion values are target values to stainless steel (SUS).

Application guidance

Application and bonding process

Bond strength depends on adhesive-to-surface contact, substrate type and surface condition. Firm pressure after assembly helps develop wet-out and engage the conductive adhesive with the substrates to establish electrical connection. Pressure, dwell time and moderate heat are process variables to evaluate for the specific assembly.

Application temperature: Tape application below 10°C (50°F) is not recommended.
Surface preparation: Bonding surfaces should be clean, dry and well unified. Isopropyl alcohol or heptane are cited as typical cleaning solvents; follow the solvent manufacturer's precautions and directions for use.
Pressure and dwell: Apply 5-15 psi after assembly using a roller, metal bar or finger pressure. A suggested initial DOE range is 5-15 psi for 2-5 seconds at 21-38°C.
Optional heat: Heat in the 38-60°C range may be applied with pressure to improve wetting, final bond strength and electrical conductivity.
Adhesion build: Up to 24-72 hours may be required to reach final adhesion values.

Firm pressure after assembly develops adhesive contact and engages the conductive adhesive with the substrates.

Storage and Handling

Shelf life is 12 months from the date of manufacture when stored in roll form, in the original packaging, at 10-25°C (50-77°F) and less than 60% relative humidity. After removal from the original packaging, converting, shipping and storage should remain within the prescribed temperature and humidity controls. If the release liner is exchanged during converting, test the replacement liner with the tape because transferred release agents can reduce tack, adhesion, electrical performance and shelf life.

Final performance

Electrical and EMI performance

Values shown are representative/typical and are not specification limits. Electrical resistance and shielding performance depend on contact and test conditions.

Property Value Unit Method / condition
Z-axis electrical resistance 0.02-0.20 Ω 3M ETM-12; 10 mm x 10 mm contact area, one pass with a 2 kg rubber roller, 20-minute dwell, then DC resistance measurement after 5-30 seconds.
Shielding effectiveness 40-60 dB Typical expected range through the tape thickness using standard EMI shielding test methods. Result depends on conductive-layer type and thickness, adhesive strength, degree of contact, surface smoothness and test frequency.
Next steps

Discuss your conductive tape application

Contact Krayden to discuss 3M-9793KW thickness and liner selection, grounding paths, surface preparation, application pressure, converting requirements and integration into EMI shielding assemblies. Provide your interface geometry and process conditions so the discussion can focus on the design and application requirements relevant to your intended use.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers